Rigorous Quality Assurance & NDT for Superalloy Castings
Inspection plans are established according to the alloy, casting route, drawing, material specification, customer requirements, and applicable acceptance criteria. ForceBeyond coordinates NDT, material verification, dimensional inspection, and documentation across the selected manufacturing route.
| Inspection Method | Purpose for Superalloys | Standard Compliance |
| Digital Radiography (X-Ray) | Detects internal microporosity and inclusions. | Per drawing / casting-specific radiography requirements |
| Fluorescent Penetrant (FPI) | Identifies surface-breaking cracks and porosity. | ASTM E1417 or applicable customer requirement |
| Ultrasonic Testing (UT) | Verifies internal density and wall thickness. | Applicable UT procedure / customer requirement |
| Spectrographic Analysis | Confirms exact chemical/alloy composition per melt. | Applicable chemistry / PMI procedure |
| CMM Dimensional Audit | Ensures tight tolerances on complex geometries. | Drawing / agreed dimensional acceptance criteria |